The onyx horizontal banding facies (2b) occurs when the ...
Description: The onyx horizontal banding facies (2b) occurs when the liquid solution has no viscosity enough to override gravity. When the polimerization of the silica solution is more viscous then the other forces active in the process causes a concentric growth (2a) or a perimetric growth (2c). image © Marco Campos-Venuti